Knit Lines and Weld Lines in Injection Molding: What to Mark on Your Drawing

Resources / Design Guides / Knit Lines and Weld Lines

Knit lines in injection molding are the thin lines you see where two flow fronts of plastic meet and fuse inside the mold. Most molded parts with a hole, a boss or more than one gate have them somewhere. You usually can’t design them out completely, but you can decide where they’re allowed to land. That decision belongs on your drawing, as cosmetic and structural zones, before the toolmaker picks a gate. This page shows how to mark those zones, what we look for in DFM, and what to check when samples arrive.

Molded plastic enclosure halves and covers in grey, white and clear on a light studio surface

Generic illustration, not a part ProteForm made.

Why does my part have a line in the same place on every shot?

Because the mold forces the flow to split and rejoin there. Molten plastic cools from the outside as it travels, so when two fronts meet, their skins don’t fully mix. You see that as a fine line, sometimes a slight groove, and on colored parts sometimes a change in shade. The usual causes:

  • Flow splits around a core pin that forms a hole, a window or a slot, then rejoins on the far side.
  • Two or more gates fill the same cavity, and their fronts meet somewhere in the middle.
  • Plastic races along a thick wall and wraps back into a thin area from the other side.
  • Flow goes around a boss, a rib intersection or an insert and closes up behind it.

A line that appears in the same spot every shot is a design and gating question, not a bad day on the press. That’s good news, because it means you can plan for it. Our guide to injection molding defects lists it alongside sink, warp and flow lines if you’re trying to tell them apart.

Mark four kinds of zone on the drawing

Toolmakers place the gate to fill the thickest section, balance flow and keep the vestige off show faces. If your drawing doesn’t say where knit lines can go, they’ll do their best guess, and the guess may not match how your customer looks at the product. We ask buyers to mark zones like these:

Zone on your drawingWhat it means to the molderTypical areasHow we review it
Cosmetic A (no visible knit line)A visible line here is a reject. Gate location and flow have to push the meeting point somewhere else.Front faces of housings, display windows, glossy or textured show surfaces, clear partsAsk for a fill study or mold-flow result showing where the fronts meet before steel is cut
Cosmetic B (faint line acceptable)A line may be visible at a stated viewing distance and light, but no groove or color streak.Side walls, lower faces, areas seen after installation but not handledAgree a limit sample at T1 so “faint” has a physical reference
Structural (no knit line in the load path)The line must not cross a feature that carries load, flexes, or holds a seal.Snap-fit roots, living hinges, screw bosses, latches, thin ribs under bendingCheck flow direction through the feature; consider moving the gate, adding a flow leader, or changing the feature
UnrestrictedKnit lines allowed. Molder uses this area to park them.Inside faces, hidden ribs, areas covered by labels or mating partsTell us this explicitly. It gives the toolmaker room to solve the zones above

You don’t need special symbols. Shaded areas on the main views with a note keyed to each shade work fine. What matters is that every face is covered by one of the four, and that at least one area is unrestricted.

Send drawings for a molded part quote with knit-line zones reviewed

Mark the cosmetic and structural zones on your drawing, or send the model and tell us which faces matter. We review gate options and likely knit-line locations with the molder in our DFM pass, and we confirm that molder before we send you a price.

Mistakes we see on drawings

Most knit-line arguments we see after sampling trace back to the drawing. These come up over and over:

  • The drawing says “no visible defects” for the whole part. That gives nobody a place to put the knit line, so the first dispute happens at T1.
  • A snap-fit hook sits right behind a hole, and the line runs straight across the hook root. On glass-filled resin that is a common place for a latch to crack.
  • Two gates are specified on the drawing by the designer to cut fill pressure, without checking where the fronts meet. The meeting point lands on the logo face.
  • A clear or high-gloss part has a window cut-out near the center. Every window makes a line on the far side, and on clear parts it is very hard to hide.
  • Texture is called out as the fix. Texture can soften how a line looks, but a deep line can still show through, and texture on a cosmetic face has its own draft needs. See how to specify texture on a drawing.
  • Nobody marks the unrestricted areas, so the toolmaker has to guess which face you care about least.

Structural zones: where a line can crack

A cosmetic line is a looks problem. A line through a latch, a hinge or a thin wall under load is a failure problem. Snap-fit hooks are the classic case: the hook flexes every time the part is assembled, and a line across its root is a weak spot. Living hinges should be filled so the flow crosses the hinge in one front, never meets in it; see living hinge design. Screw bosses near a hole often get a line down one side, which can split when the screw goes in.

The fixes, in rough order of cost: move the gate so the meeting point lands outside the feature; add a flow leader (a slightly thicker path in the wall) to steer the front; add a vent or overflow well at the meeting point so the fronts meet hotter and cleaner; change the feature, for example move the hole away from the latch. Some of these change your part geometry, so they come back to you as DFM questions. If you’re designing latches now, snap-fit design is worth reading alongside this page.

Glass-filled and mineral-filled grades deserve extra care. Fibers line up with the flow and don’t bridge the knit line well, so a feature that tests fine in an unfilled sample can behave differently in the filled production resin. If you’re moving to a filled grade, review structural zones again. See glass-filled nylon injection molding.

What happens from DFM to approved sample

1

Before the gate is set

Send the drawing with zones marked. In the DFM report, look for the proposed gate location and a statement of where knit lines are expected. On cosmetic or load-bearing parts, a fill simulation is worth asking for. Our page on mold-flow analysis covers what the report should show you.

2

At T1 samples

Look at the zones you marked, in the light and at the distance your customer will use. Bend or load test any structural feature near a line. Photograph each line with a ruler or a marked location so the molder knows exactly which one you mean. Put that viewing distance and light into your written cosmetic inspection criteria, so the molder’s inspectors check the part the way you do.

3

If a line is in the wrong place

Process changes such as melt temperature, mold temperature and injection speed can make a line fainter and stronger. They rarely move it far. Moving it usually means a gate change, a flow leader added to the wall, or a vent at the meeting point, which are tool changes with cost and time.

4

Before you approve

Sign a limit sample for every Cosmetic B zone and keep one at both ends. Our sample approval and first article guide covers how to record it.

Multi-cavity tools add one more check. Each cavity has its own gate and fill pattern, so a line can look acceptable in cavity 1 and not in cavity 4. Ask for samples from every cavity, marked by cavity number, before you sign off.

Frequently asked questions

Are knit lines and weld lines the same thing?

In most shops, yes. Some engineers use “knit line” for fronts that meet head-on and “meld line” for fronts that meet while still flowing side by side, which usually blends better. On a drawing or in a quote, treat them as the same issue and describe where they are and are not allowed.

Can a knit line be removed completely?

Only if the flow never splits, which is rare once a part has holes or more than one gate. What you can control is where the line lands and how visible and strong it is. Gate location does most of that work; processing fine-tunes it.

Are knit lines weaker than the rest of the part?

They can be, and the drop is usually worse in glass-filled resins, because fibers do not cross the line well. How much weaker depends on the resin, the process and how the fronts meet. If a feature is load-bearing, keep the line out of it and test samples rather than relying on a general figure.

How should I write a knit-line note on a drawing?

Mark zones on the part views and add a short note for each, for example: cosmetic zone, no visible knit line; secondary zone, faint line acceptable per limit sample; structural zone, no knit line across the feature. Leave at least one area unrestricted so the toolmaker has somewhere to put them.

Will texture or paint hide a knit line?

Sometimes. A light texture or a painted finish can make a shallow line hard to see, but a groove or a color streak can still show, especially on dark or metallic colors. Effect pigments tend to make lines more obvious. Agree the finish and the zone together, then check it at T1. See painting molded plastic parts.

Send drawings for an injection molding quote

Send STEP files, the drawing with zones marked if you have them, resin and color, annual volume, and any photos of lines you have rejected on a previous supplier’s parts. We come back with DFM questions first, name the supplier we would use, and quote once the gate and cosmetic plan is agreed.

Send us your drawing

A real engineer reads every request and comes back with questions or a plan for quoting.

ProteForm short RFQ

Or message us on WhatsApp.

Send Drawings
Chat on WhatsApp