The gate is the opening through which molten plastic enters the part cavity. Its type, size and location affect how the part fills, where weld lines and air traps form, how well thick areas pack, how the part warps, and what mark is left on the surface. Gate decisions are made by the toolmaker, but buyers and designers should understand them, because they affect appearance and performance and are hard to change after the tool is cut. This guide explains common gate types, how gate location is chosen, and what to tell your supplier.
Common gate types
| Gate type | How it works | Typical use | Gate mark |
|---|---|---|---|
| Edge (tab) gate | Enters the part at the parting line from the side | General parts; simple and common | Visible vestige on an edge; trimmed after molding |
| Submarine (tunnel) gate | Tunnel below the parting line, sheared off at ejection | Automatic degating of small parts | Small mark on a side or hidden face |
| Pin-point gate (three-plate mold) | Small gate from above, broken off as the mold opens | Gating on a face, center of round parts | Small dot on the face |
| Hot runner tip / valve gate | Plastic stays molten up to the gate; valve gates close mechanically | High volume, large parts, reduced runner waste | Small ring or dot; valve gates are cleanest |
| Fan gate | Wide, thin gate spreading flow | Flat parts, reduced flow lines and warp | Long edge vestige that must be trimmed |
| Film (flash) gate | Very thin gate along an edge | Thin flat parts, clear parts | Long edge vestige |
| Diaphragm / ring gate | Fills round parts evenly from the center or around the edge | Tubes, round parts needing concentricity | Ring or disc removed after molding |
| Direct (sprue) gate | Sprue feeds the part directly | Large single-cavity parts, prototypes | Large vestige where the sprue is removed |
How gate location is chosen
- Fill into the thickest section. Plastic should flow from thick to thin, so thick areas can be packed before the gate freezes. Gating into a thin area starves thick sections and causes sink and voids.
- Balanced flow. The gate should allow all extremities to fill at about the same time, avoiding over-packing near the gate and short shots far away.
- Weld lines in harmless places. Where flow fronts meet around holes or from multiple gates, weld lines form. Gate location moves them away from cosmetic faces and high-stress areas; see knit lines and weld lines for how to mark those zones on your drawing.
- Venting. The last area to fill must be vented, or trapped air causes burns and short shots.
- Cosmetics. The gate vestige should fall on a non-cosmetic face or edge.
- Fiber orientation and warp. In filled resins, fibers align with flow; gate location affects shrinkage direction and warp.
- Living hinges and thin features. Flow should cross hinges in one front; see living hinge design.
Gate size
Gates that are too small freeze early, preventing packing and causing sink, and can shear-heat the plastic, degrading it. Gates that are too large leave large vestiges and can take longer to freeze. Toolmakers often cut gates slightly small and open them up after the first trials, because enlarging steel is easy and reducing it is not. Resin suppliers publish gate size guidance for their materials.
Send CAD for a gate and DFM review
Cold runner vs hot runner
| Aspect | Cold runner | Hot runner |
|---|---|---|
| Tool cost | Lower | Higher; adds manifold and controllers |
| Material waste | Runner is scrap or regrind | Little or no runner waste |
| Cycle time | Runner must cool | Often shorter |
| Color changes | Easy | Slower; material must purge from manifold |
| Gate options | Edge, sub, pin-point (three-plate) | Open tips, valve gates |
| Best for | Low to medium volume, frequent color changes | High volume, large parts, expensive resins |
The choice affects tooling cost and unit price; see hot runner vs cold runner and tooling cost vs unit price.
Multiple gates
Large or long parts may need more than one gate to fill within reasonable pressure. Each extra gate creates weld lines where the flow fronts meet. Valve gates can be opened in sequence (sequential valve gating) so the flow front moves through the part without forming weld lines in critical areas. Multi-gate decisions are usually checked with mold-flow simulation; see mold-flow analysis.
What the gate means for appearance
- Edge and fan gates leave a vestige that is trimmed, often leaving a small mark or rough spot.
- Sub gates leave a small mark that is usually acceptable on hidden faces.
- Pin-point and hot tip gates leave a small dot or ring, sometimes slightly raised; valve gates are the cleanest.
- Flow lines, jetting and blush near the gate are processing and gate-design issues; see molding defects.
On cosmetic parts, mark on the drawing where gate vestiges are and are not allowed, and the maximum allowed vestige height.
Gates in multi-cavity and family tools
In a multi-cavity tool, each cavity has its own gate, and the runner must deliver plastic to every cavity at the same pressure and temperature. Runners are usually laid out to be naturally balanced, with equal flow lengths to every cavity. If they are not, cavities near the sprue fill first and pack harder, so parts from different cavities differ in size and weight. Family tools that mold different parts together are harder to balance, because each part needs a different amount of plastic. Ask for cavity-by-cavity dimensional data at first samples, not only one part.
Degating and trimming
Some gates separate automatically (sub gates, pin-point gates, hot tips); others must be cut by hand or with a fixture after molding (edge, fan, film and diaphragm gates). Manual degating adds labor and variation, and can leave stress or whitening at the gate. For high volumes, self-degating designs or robotic trimming reduce cost. Ask how the gate will be removed and what finish is expected at the cut.
Gates in other processes, compared
| Process | Equivalent consideration |
|---|---|
| Vacuum casting | Pour and vent locations in the silicone mold |
| LSR molding | Cold-runner gating; valve gates common to avoid flash |
| Compression molding | No gate; charge placement instead |
| Rotational molding | No gate; powder distribution by rotation |
What to tell your supplier
- Which faces are cosmetic and where gate marks must not appear.
- Areas where weld lines are unacceptable for strength or appearance.
- Critical dimensions and flatness, so gate location can minimize warp there.
- Expected annual volume, to guide cold vs hot runner.
- Color change frequency.
- Ask for the proposed gate location and type in the DFM report, ideally with a mold-flow result.
Frequently asked questions
What is a gate in injection molding?
The opening through which molten plastic enters the part cavity from the runner.
Where should the gate be located?
Usually into the thickest section, positioned for balanced fill, with weld lines and the gate mark in non-critical areas.
What is the difference between a sub gate and an edge gate?
An edge gate enters at the parting line and is trimmed; a sub gate tunnels below the parting line and shears off automatically at ejection.
Are hot runners always better?
No. They reduce waste and cycle time but cost more and make color changes slower. They suit high volumes.
Can the gate be moved after the tool is built?
Sometimes, but it can be costly. Agree gate location in the DFM review before steel is cut.