Custom Overmolding Services: TPE and TPU Over Plastic or Metal

You have a rigid part that needs a soft grip, a seal, or a bumper, and you’re tired of gluing a rubber piece on by hand. Our custom overmolding services cover the usual routes: a soft TPE or TPU layer molded onto a plastic substrate, two-shot (2K) molding in one tool, and plastic molded over metal inserts. We review the drawing first, agree which shop makes it, then quote.

Soft-touch overmolded handle grip next to black and translucent elastomer seals and gaskets on a gray surface
Illustrative photo of soft-touch and elastomer parts. Not a customer part.

What does overmolding actually involve?

Overmolding means molding one material onto a part that already exists. The first part is called the substrate. It’s usually a rigid plastic such as PP, ABS, PC, PC/ABS or nylon, and sometimes a metal stamping, a threaded insert, or a machined shaft. The second material is usually softer: a thermoplastic elastomer (TPE), TPU, or in some cases liquid silicone rubber.

The two layers stay together in one of two ways. Either the soft material is chosen to bond chemically to that specific substrate, or the substrate is designed with holes, grooves or undercuts so the soft layer locks on mechanically. Most good designs use both. If you’re relying on chemistry alone, the material pairing has to be right, and that’s the first thing we check on your drawing.

Two-shot molding or pick-and-place overmolding: which one fits your part?

This choice drives most of your tooling cost, so it’s worth settling early. In two-shot (2K) molding, one press with two injection units shoots the rigid material, then the mold rotates or transfers the part and shoots the soft material. You get a finished part every cycle. The tooling is more complex and fewer shops run it, so it makes sense when volumes are steady and high enough to pay for that tool.

In pick-and-place overmolding, the substrate is molded in one tool, then loaded by hand or by robot into a second tool where the soft layer goes on. Two simpler molds instead of one complex one. You pay for it in handling time per part and in more chances for the substrate to be loaded wrong or to pick up dust or oil before the second shot. For pilot runs and moderate volumes it’s often the sensible start.

Route How it works Usually fits when Watch out for
Two-shot (2K) moldingBoth materials shot in one tool on a two-barrel press.Stable design, steady volume, tight registration between the layers.Highest tooling cost; design changes after steel is cut are expensive; fewer shops to choose from.
Pick-and-place overmoldingSubstrate molded first, then loaded into a second mold for the soft layer.Pilot runs, moderate volume, designs still settling.Labor per part, loading errors, contamination on the substrate before the second shot.
Insert molding over metalMetal inserts, pins or stampings placed in the mold and plastic shot around them.Threaded inserts, contacts, shafts, reinforced brackets.Insert tolerance and cleanliness, flash around the insert, insert supply as a separate purchase.
Separate soft part, assembledSoft part molded on its own, then pressed, clipped or glued on.Low volume, a replaceable grip or seal, or a pairing that won’t bond.Assembly labor, gaps or lifting edges, adhesive aging.

If you can’t tell yet which route you need, say so in the RFQ. Give us your expected annual quantity and how sure you are of it, and we’ll lay out the options. The injection molding MOQ guide explains why low or uncertain volume changes the answer.

Which TPE or TPU will actually bond to your substrate?

Not every soft grade sticks to every rigid plastic. TPE suppliers sell grades formulated for adhesion to particular substrates, for example one family for PP and a different one for PC, ABS or nylon. If you pick a soft grade from a hardness chart without checking the substrate, the grip may peel at the first drop test. TPU tends to be chosen where abrasion, oil or tear resistance matters more than a silky feel. Silicone over plastic needs self-bonding LSR grades and a substrate that can take the cure temperature, so it’s a narrower path.

On the drawing or in the RFQ, give us the substrate material (grade if you have one), the soft material and hardness you want, usually as a Shore A value, color for both layers, and what the part touches in use: hand sweat, cleaning agents, oil, UV, hot water. That’s how we and the molding shop shortlist grades. If you already have a grade from your previous supplier, send it. We’ll tell you if the pairing worries us. Our elastomers page and engineering plastics page cover the families in more detail.

Nylon substrates deserve a separate mention. Nylon absorbs moisture, and a wet substrate can bond poorly. If your rigid part is PA6 or PA66, especially glass-filled, read what to specify for glass-filled nylon injection molding before you lock the material.

Send drawings for an overmolding quote

Send the substrate and overmold CAD (STEP is best), a 2D drawing with critical dimensions, both materials or the properties you need, Shore hardness, colors, and your expected yearly quantity. We’ll review it for moldability, confirm which shop would build and run the tools, and only then send a quote.

What design details cause overmolding problems at sampling?

Most first-sample complaints trace back to things you can see on the CAD before steel is cut.

Shut-off edges

The soft material has to stop somewhere, and the mold stops it by clamping against the substrate. If that edge is a thin feather or sits on a curved surface with loose tolerance, you get flash. A small step or groove in the substrate where the soft layer ends gives the tool something firm to seal against.

Soft layer thickness

Very thin soft layers are hard to fill and tend to peel at the edges. Very thick ones sink and take longer to cool. Keep the soft layer as even as you can, and expect the shop to suggest changes after a fill check.

Mechanical lock

Even with a bonding grade, through-holes, undercuts or a groove the soft layer wraps into will help when the part is twisted, pulled or dropped. On grips and bumpers we’ll usually ask for one.

Substrate tolerance

In pick-and-place work the substrate has to sit in the second tool the same way every time. If it varies, the shut-off varies, and so does the flash. That means the substrate dimensions matter more than they would on a standalone part.

Gate marks and cosmetics

Tell us which faces are cosmetic. The soft layer gate has to go somewhere, and on a grip you don’t want it where the thumb sits.

More on walls, draft and ribs is in the design guides.

What happens between RFQ and approved samples?

We read the drawing and send back questions: material pairing, shut-off, lock features, cosmetic faces, and whatever on the drawing doesn’t match the 3D model. Once the design is agreed, we confirm the shop that will build and run the molds, and that name goes into our quote. You won’t get a quote from us that’s based on a guess about who might make it.

At sampling, ask for more than photos. Useful checks include a peel or pull test agreed in advance, flash at the shut-off line, color match on both layers, and dimensions on the features that mate with other parts. If you need a formal report or first-article inspection, name it in the RFQ so it’s part of the quote. Our quality approach explains how inspection is agreed per job.

Tooling ownership deserves the same attention as on any molded part, with one wrinkle: overmolding usually means two molds or one complex 2K tool. Write both into the order. Our guide on who owns the mold covers what to put in writing.

Where do buyers use overmolded parts?

Common jobs include soft-touch grips on hand tools and handheld devices, sealing lips on enclosures, bumpers and feet on robotics and industrial equipment covers, cable strain reliefs, buttons and keypads in consumer electronics, and interior trim details in automotive programs. If the overmolded part goes into a larger product, we can also handle the steps after molding through finished assembly and secondary operations such as pad printing or ultrasonic welding.

When are we not the right fit for overmolding?

If you need a handful of soft-grip prototypes next week, a mold is the wrong answer. Look at 3D printing or a cast urethane over a printed core first, and come back to overmolding when the design stops moving. We’re also not the right choice if you already run a 2K program with a shop you trust and only want the lowest piece price on a re-quote.

We’re most useful when you have a design, aren’t sure which route or pairing makes sense, and want a capable shop confirmed before money goes into steel.

What should your overmolding RFQ include?

  • 3D CAD for the substrate and the overmold, as separate bodies if you can, plus a 2D drawing with critical dimensions and tolerances.
  • Substrate material and the soft material, with grade names if you have them, Shore hardness, and colors.
  • What the part has to survive: drop, pull, cleaning chemicals, oil, UV, temperature.
  • Cosmetic faces, texture, and where a gate mark is not acceptable.
  • Expected annual quantity, first order quantity, and how firm those numbers are.
  • Inspection or documents you need with samples and shipments.
  • Any existing tooling, and who owns it.

The general RFQ checklist covers the rest.

Frequently asked questions

What is the difference between overmolding and two-shot molding?

Two-shot molding is one way to overmold. Both materials are shot in a single tool on a press with two injection units. Overmolding is the broader term and also covers pick-and-place, where the rigid part is molded first and then loaded into a second mold for the soft layer. Two-shot costs more to tool and suits steady volume; pick-and-place uses simpler molds but more handling per part.

Can TPE be overmolded onto nylon or polycarbonate?

Yes, with TPE grades made to bond to that substrate. A grade that bonds well to PP won’t necessarily stick to PC or nylon. Send us the substrate material and grade, and we’ll shortlist soft grades with the molding shop. For nylon, the substrate also needs to be dry when it’s overmolded.

How do you check that the soft layer won’t peel off?

Agree the test before sampling. That can be a pull or peel test, or a hand peel judged against an approved reference sample, plus a check after any conditioning you care about, such as heat or a cleaning agent. Good design helps too: a groove, undercut or through-hole for a mechanical lock gives a margin if adhesion is weaker than expected.

Is overmolding worth it at low volume?

Sometimes not. At low or uncertain volume, a separately molded or cast soft part that’s pressed or bonded on can cost less in total, because you avoid a second mold or a 2K tool. Tell us your realistic quantity and we’ll compare the routes honestly rather than default to overmolding.

Can you overmold plastic onto metal inserts?

Yes, that’s insert molding. Threaded inserts, pins, contacts and stamped brackets are common. Tell us who supplies the inserts, the insert drawing and tolerance, and how they’ll be cleaned and loaded, because insert variation shows up as flash or poor retention in the molded part.

Send drawings for an overmolding quote

Send substrate and overmold CAD, a 2D drawing, both materials, hardness, colors, and your realistic yearly quantity. We’ll review the design, tell you which route we’d use and why, agree which shop makes it, then quote. We don’t do instant quotes, and if overmolding isn’t the right call for your volume, we’ll say so.

Send us your drawing

A real engineer reads every request and comes back with questions or a plan for quoting.

ProteForm short RFQ

Or message us on WhatsApp.

Send Drawings
Chat on WhatsApp