Custom manufacturing support for product teams worldwide Discuss Your Project  →

Liquid Silicone Rubber (LSR) Molding for Seals, Gaskets and Soft Parts

Capabilities / Injection Molding / Liquid Silicone Rubber Molding

You need a seal, gasket, membrane, button pad or soft cover that stays flexible across heat and cold, doesn’t take a set after being squeezed for months, and looks the same from the first part to the last. That usually points to silicone, and for repeat parts it often points to liquid silicone rubber (LSR) molding. We review your drawing and the use conditions first, confirm the shop that will build the tool and mold the parts, and then quote.

Translucent molded silicone seals and gaskets with flexible soft parts on a cool gray surface

What is liquid silicone rubber molding?

LSR is a two-part, platinum-cured silicone that comes as a paste. The two components are metered, mixed and injected into a heated mold, where the material cures into a solid rubber part. That is the opposite of a thermoplastic, which is melted hot and frozen in a cold mold. Because the material is runny before it cures, it fills thin walls and fine detail well. It also flashes into any gap in the tool, which is why LSR molds need tight shut-offs.

The finished parts keep their properties across a wide temperature range, resist ozone and UV well, and recover after compression. Translucent and colored grades are common. These are family traits, not promises for every grade, so the exact grade and its data sheet are confirmed per project.

LSR, compression-molded silicone or TPE: which one fits your part?

Before choosing LSR, check whether one of the alternatives does the job. The answer depends on the quantity, the shape and what the part has to survive.

Option Good for Watch out for
LSR injection moldingRepeat silicone parts, thin walls, fine detail, consistent quality, two-shot with plastic.Tool is more complex and costly than a compression mold; flash control needs a well-made tool; volume has to justify it.
Compression-molded silicone (HCR)Larger, simpler silicone parts, lower quantities, cheaper tooling.More manual work per part, more trimming, wider variation than LSR.
TPE or TPU injection moldingSoft parts where silicone’s temperature range isn’t needed; can be recycled; easy two-material molding.Lower heat resistance and more compression set than silicone in many grades; check the grade against your conditions.
Cast or 3D-printed silicone prototypesA handful of parts to check fit and feel.Properties differ from molded LSR; fine for fit checks, not for final validation.

If the part is a soft grip or seal on a rigid housing, also read our page on overmolding. If you are still comparing soft materials, our elastomers page covers TPE, TPU, silicone and rubber as families.

What should you design differently for LSR?

Silicone is soft and stretchy, which changes several rules you may know from rigid plastic parts.

Undercuts are easier. A cured silicone part can often be stretched off a core, so undercuts that would need side actions in a rigid part may demold without them. How far you can go depends on the hardness and the geometry; the molder will confirm it on your part.

Flash is the main risk. LSR finds gaps that a thermoplastic would not. Put parting lines where a small flash line doesn’t matter, and tell us which edges are sealing or cosmetic. A sealing lip with flash across it is a reject.

Shrinkage is different. Silicone shrinks as it cools out of a hot mold, and post-cure can change it further. Don’t copy shrink factors from a thermoplastic drawing. Tolerances on soft parts are also harder to measure, because the part deforms when you touch it. Agree how each critical dimension will be measured: with a fixture, an optical system, or on the mating part.

Hardness and feel. Specify hardness as a Shore A value with a tolerance, and say what the part has to do: seal at a given compression, give a certain button feel, or survive a number of cycles. If you don’t know the hardness yet, describe the function and we’ll ask the molder what grades they would try.

Send drawings for an LSR molding quote

How does the tooling work, and what drives the cost?

An LSR mold is heated, often with a cold runner or valve-gated system that keeps the material uncured until it reaches the cavity. That reduces waste because silicone runners can’t be reground. Tight steel fits, venting and good shut-offs are what stop flash, and they are a large part of the tool price. Demolding is often by hand, air or brush on smaller programs, and automated on high-volume ones.

For early parts, some shops cut a simpler prototype mold to check the design before the production tool. Ask for it if your geometry is still moving. The cost conversation then becomes: how many changes do you expect, and how soon will volume be stable? Our guide on what drives injection mold cost covers the general drivers, and most of them apply to LSR too.

Post-cure, cleanliness and documents

Many LSR parts are post-cured in an oven after molding to drive off volatile compounds and stabilize properties. Whether you need it depends on the grade and the application. If the part touches food, skin or sensitive electronics, ask for it explicitly and agree how it’s done and recorded.

Food-contact, skin-contact and other compliance statements belong to a specific grade from a specific material supplier, processed in a certain way. We don’t treat them as family-level claims. Tell us which documents you need, and we’ll confirm what the material supplier and the molding shop can provide before quoting. If a regulated medical device is involved, say so at the start; some programs need a shop with approvals we may not be able to confirm.

Can LSR be molded onto plastic in one part?

Yes. Self-bonding LSR grades can be molded onto a rigid substrate such as PC, PBT or nylon, either in a two-shot process or by placing a pre-molded plastic part in the LSR mold. The substrate has to handle the mold temperature, and the bond depends on the pairing of grade and substrate. Mechanical interlocks such as holes and grooves help even when the grade bonds chemically. That route is close to what our overmolding page describes for TPE, with tighter limits on substrate choice.

How do you check molded silicone parts?

Agree the checks before sampling. Typical ones are hardness on a test piece or the part, visual checks for flash, voids, bubbles and contamination, dimensional checks with an agreed fixture or optical method, and a function test such as a compression or leak test for seals. Keep signed limit samples for flash and cosmetic defects, because “no visible flash” means different things to different inspectors. Our quality approach explains how inspection is agreed per project.

When are we not the right fit?

If you need silicone parts for an implantable or invasive medical device, you need a molder with the specific approvals and clean-room setup for that work, and you should go to one directly. If you need a few prototype gaskets in days, a local silicone caster will be faster. We’re most useful when you have a defined silicone part, a real production quantity in view, and you want someone to check the design and confirm the shop before you pay for a tool.

What should your LSR molding RFQ include?

  • 3D CAD and a 2D drawing with critical dimensions, tolerances and how each one will be measured.
  • Hardness (Shore A) with tolerance, color, and translucency if it matters.
  • Use conditions: temperature range, fluids or chemicals, UV exposure, compression or cycle life.
  • Sealing and cosmetic edges, and where flash or parting lines are acceptable.
  • Any substrate if the silicone goes onto plastic or metal.
  • Documents you need, such as material data sheets or food-contact statements, and whether post-cure is required.
  • Expected annual quantity, first order quantity, and how firm those numbers are.
  • Packing requirements; silicone picks up dust and lint easily. A blank RFQ checklist is on our downloads page.

Frequently asked questions

What is the difference between LSR and HCR silicone?

LSR is a liquid, two-part silicone that is injection molded into a heated tool. HCR (high consistency rubber) is a stiffer, gum-like silicone usually compression or transfer molded. LSR suits repeat parts with thin walls and fine detail; HCR often suits larger, simpler parts and lower quantities with cheaper tooling.

Is LSR better than TPE for seals?

For seals that see high or low temperatures, long-term compression or outdoor exposure, silicone often performs better than many TPE grades. TPE can be cheaper, recyclable and easier to mold onto plastic. The right choice depends on the conditions; send them and we will compare both.

Can you mold LSR in different colors or clear?

Yes. LSR is commonly molded translucent or pigmented to a color reference. Agree the color standard and a master sample before production, since color on soft parts is also judged against a physical reference.

Do LSR parts need post-curing?

It depends on the grade and the application. Post-cure is common when parts touch food or skin, or sit near sensitive electronics. Ask for it in the RFQ and agree how it is done and recorded.

Can silicone be bonded to a plastic housing in the mold?

Yes, with self-bonding LSR grades and a substrate that can take the mold temperature, such as some PC, PBT or nylon grades. The pairing has to be confirmed with the material supplier and the molder before the tool is built.

Send drawings for an LSR molding quote

Send us your drawing

A real engineer reads every request and comes back with questions or a plan for quoting.

ProteForm short RFQ

Or message us on WhatsApp.

Send Drawings
Chat on WhatsApp