POM (acetal) and PTFE are both chosen for low friction, so they often end up on the same shortlist for bushings, bearings, slides, seals and valve parts. They behave very differently. POM is a stiff, strong, dimensionally stable engineering plastic that machines beautifully and can be injection molded. PTFE has one of the lowest friction coefficients of any solid, resists almost every chemical and handles far higher temperatures, but it is soft, creeps under load and cannot be molded like ordinary thermoplastics. This comparison explains the differences in mechanical behavior, friction and wear, temperature, chemical resistance, processing, cost and where each is typically used, so you can tell which one the part actually needs.
Quick comparison
| Property | POM (acetal) | PTFE |
|---|---|---|
| Type | Semi-crystalline engineering thermoplastic | Fluoropolymer |
| Stiffness and strength | High; holds shape under load | Low; soft and flexible |
| Creep (cold flow) | Low | High, especially unfilled |
| Friction | Low | Very low; among the lowest of solids |
| Wear resistance | Good against metal | Poor unfilled; much better with fillers |
| Continuous service temperature | Moderate; well below PTFE | Very high, roughly up to about 260 °C |
| Chemical resistance | Good to solvents and fuels; attacked by strong acids and oxidizers | Resists almost all chemicals |
| Moisture absorption | Low | Negligible |
| Processing | Injection molding, extrusion, machining | Compression molding and sintering, ram extrusion, skiving, machining |
| Density | Lower | Much higher, roughly 2.1–2.2 g/cm³ |
| Relative cost | Moderate | Higher |
Exact values vary by grade, filler and supplier; use the data sheet for the specific grade, measured by the same test method, when comparing.
Mechanical behavior
POM is one of the stiffest unfilled thermoplastics, with good strength, fatigue resistance and spring-back. That is why it is used for gears, snap fits, clips and precision mechanical parts that must hold dimensions under load. PTFE is soft. Under steady load it slowly deforms, called creep or cold flow, which can loosen press fits, flatten seals and change clearances. Filled PTFE grades, with glass, carbon, graphite or bronze, are much better in creep and wear, though still not as rigid as POM. If a part carries structural load or needs tight dimensional stability, POM is usually the safer starting point.
Grades within each family
Acetal comes as homopolymer (often sold under the Delrin name) and copolymer grades. Homopolymer is typically a little stiffer and stronger; copolymer typically has better resistance to hot water and alkaline conditions and less centerline porosity in thick stock. PTFE comes as virgin (unfilled) grades, preferred for chemical purity and electrical uses, and filled grades with glass, carbon, graphite, bronze or polymer fillers that improve creep and wear at the cost of some chemical and electrical performance. Comparing the right sub-grade matters as much as comparing the families.
Friction and wear
Both have low friction, but PTFE is lower and has little difference between static and dynamic friction, so it does not stick-slip. Unfilled PTFE wears quickly in sliding contact, so bearing grades are almost always filled. POM has a good balance of low friction and wear resistance against metal and runs well unlubricated at moderate loads and speeds. For a heavily loaded, low-speed bushing in a dry environment, POM often works; for very low friction, high temperature or chemical exposure, filled PTFE may be needed. Compare PTFE vs UHMW-PE and acetal vs nylon for other low-friction options.
Send your part for a material review
Temperature
PTFE remains usable across a very wide temperature range, from cryogenic conditions to roughly 260 °C in continuous service. POM’s continuous service temperature is much lower, and it loses stiffness as temperature rises; it also degrades if overheated during processing. For hot environments, PTFE or other high-performance plastics such as PEEK are typical choices; see PEEK vs PTFE.
Chemical resistance
PTFE is resistant to nearly all industrial chemicals, which is why it is used in seals, linings and valve seats in chemical handling. POM resists many solvents, fuels and oils well, but it is attacked by strong acids, strong bases in some conditions and oxidizing agents, and chlorinated water can be a concern for some grades. If the part sees aggressive chemicals, PTFE or another fluoropolymer such as PVDF is usually considered first. Always check the specific chemical, concentration and temperature against supplier compatibility data.
Processing and manufacturing
POM is a conventional thermoplastic: it injection molds well, with good flow and fast cycles, and extruded rod and plate machine very cleanly with tight tolerances. It shrinks more than many amorphous resins, so molded part design must allow for that. PTFE has such a high melt viscosity that it cannot be injection molded in the normal way. It is compression molded and sintered into billets, ram extruded into rods and tubes, or skived into film; parts are then machined. Melt-processable fluoropolymers such as PFA and FEP exist when molded fluoropolymer parts are needed. PTFE is soft and springy to machine, and tolerances need to account for its high thermal expansion and creep. See CNC machining.
Bonding and assembly
Both have low surface energy and are hard to bond with adhesives. PTFE usually needs chemical etching or plasma treatment; POM needs surface treatment or special primers. Mechanical retention, press fits (allowing for PTFE creep), snap fits in POM and threaded fasteners are more common. See adhesive bonding of plastics.
Where each is typically used
| Application | POM | PTFE |
|---|---|---|
| Gears, cams, clips, snap fits | Typical choice | Rarely; too soft |
| Bushings and bearings | Moderate loads, dry running | Filled grades; high temperature or chemicals |
| Seals, gaskets, valve seats | Some low-pressure uses | Typical choice, especially chemical service |
| Slides and wear strips | Common | Filled grades; very low friction needs |
| Chemical linings and piping components | Rarely | Typical choice |
| Electrical insulators | Some uses | Excellent dielectric properties; high-frequency uses |
| Food-contact parts | Food-contact grades available | Food-contact grades available |
Food-contact and other regulatory status depends on the specific grade and its documentation; confirm with the resin supplier.
Cost
PTFE stock is generally more expensive than POM by volume, and its higher density increases cost per part further. Machining time and scrap can also be higher. POM can be molded at volume, which makes it far cheaper for high-quantity parts. Choose PTFE when its temperature, chemical or friction properties are genuinely needed, not by default.
How to choose
- Structural load, stiffness or tight tolerances: start with POM.
- Very high temperature or aggressive chemicals: start with PTFE.
- Very low friction with no stick-slip: PTFE, filled for wear.
- High volume and moldability: POM.
- Seals and gaskets that must conform: PTFE.
- Unsure: list load, speed, temperature, chemicals and quantity, and ask for a review.
See the engineering plastics and high-performance plastics hubs, and the acetal (POM) and PTFE material pages.
Frequently asked questions
Is POM or PTFE better for bushings?
POM suits moderate loads and temperatures with good dimensional stability. Filled PTFE suits high temperatures, chemicals or very low friction.
Can PTFE be injection molded?
Not conventionally. PTFE is compression molded and sintered, ram extruded or skived, then machined. PFA and FEP are melt-processable alternatives.
Which has lower friction, acetal or PTFE?
PTFE has lower friction and no stick-slip, but unfilled PTFE wears quickly.
Is acetal chemically resistant?
It resists many solvents, fuels and oils, but strong acids and oxidizing agents attack it. PTFE resists almost all chemicals.
Which is cheaper, POM or PTFE?
POM is generally cheaper and can be molded at volume; PTFE costs more per part.