acetal (POM) and nylon (PA) are the two engineering plastics most often considered for gears, bushings, rollers, clips and wear parts. Both are strong, tough and slippery compared with commodity plastics, and both machine and mold well. The main differences are moisture, dimensional stability, toughness, temperature and chemical resistance. This guide compares them for machined and molded parts and explains how to choose. Acetal is often sold as Delrin (homopolymer) or under various copolymer trade names; nylon as PA6, PA66 and cast nylon.
Quick comparison
| Property | Acetal (POM) | Nylon (PA6 / PA66) |
|---|---|---|
| Moisture absorption | Very low | Significant; properties and size change with humidity |
| Dimensional stability | Excellent; holds tight tolerances | Lower; grows as it absorbs moisture |
| Stiffness | High | High when dry, lower when conditioned |
| Toughness and impact | Good | Very good, especially when conditioned |
| Friction and wear | Low friction, smooth sliding | Good wear and abrasion resistance; lubricated grades available |
| Temperature resistance | Moderate | Higher, especially PA66 and glass-filled grades |
| Chemical resistance | Good with fuels, solvents and oils; attacked by strong acids and oxidizers | Good with oils, fuels and many solvents; attacked by strong acids |
| Glass-filled grades | Available but less common | Very common for structural parts |
| Bonding and painting | Difficult | Easier than acetal |
Moisture and dimensional stability
This is usually the deciding factor. Acetal absorbs very little water, so a part machined or molded to size stays there in humid air or in contact with water. Nylon absorbs moisture and grows slightly; it also becomes tougher and less stiff as it does. For precision parts such as small gears, valve components, fixtures and close-fitting assemblies in changing humidity, acetal is often the safer choice. Nylon can still be used if clearances and tolerances allow for its movement. See nylon machining for how this affects machined parts.
Wear, friction and gears
Both are classic gear and bearing materials. Acetal has low friction and runs smoothly against steel and against nylon; acetal-on-nylon gear pairs are common because the combination wears well. Nylon resists abrasion in dirty environments and absorbs shock loads, which suits rollers, wear pads and heavy-duty gears. Lubricated grades of both exist: PTFE-filled acetal, oil-filled and MoS2-filled nylon.
Temperature and strength
Nylon, especially PA66 and glass-filled grades, handles higher temperatures than acetal and is common under the hood, near motors and in structural brackets. Acetal is suited to moderate temperatures. For parts that combine heat and structural load, glass-filled nylon is a frequent choice; see our glass-filled nylon guide.
Get a quote in acetal or nylon
Chemicals
Both resist oils, greases and many fuels and solvents. Acetal is degraded by strong acids and oxidizing agents, including some chlorinated cleaning agents; nylon is also attacked by strong acids. Hot water over long periods can affect both, and some acetal grades are specifically formulated for hot water. Name the fluids and temperatures so the supplier can suggest a grade.
Machining and molding
- Machining: acetal is one of the easiest plastics to machine to tight tolerance with clean edges. Nylon machines well but leaves more burrs and can move with moisture and stress.
- Molding: both mold well. Acetal is prone to sink in thick sections and needs good venting; nylon needs drying and care with moisture after molding. Both shrink more than amorphous plastics, which tools must allow for.
- Homopolymer vs copolymer acetal: homopolymer is generally stiffer and stronger; copolymer has better resistance to hot water and some chemicals and less centerline porosity in thick stock.
Cost and availability
Both are widely available as rod, plate and molding resin. Nylon is usually a little cheaper per kilogram in unfilled grades, and cast nylon is available in very large sizes that acetal is not. Acetal stock in large diameters can have centerline porosity, especially homopolymer, which matters for parts machined from the center of thick rod. For molded parts, resin price differences are often smaller than the effect of cycle time and scrap.
Electrical and other properties
Both are good electrical insulators, but nylon’s electrical properties change with moisture content, while acetal’s stay more stable. Both are available in food-contact grades and in colors; confirm documentation for the specific grade if food contact or a regulatory listing applies. Neither is suited to long outdoor exposure without UV stabilization; black grades with carbon black hold up better.
Switching from one to the other
Buyers sometimes switch a nylon part to acetal to fix dimensional drift, or an acetal part to nylon for toughness or heat. For machined parts this is usually simple: re-cut from the other stock and retest. For molded parts, the two resins shrink differently, so an existing mold may not produce in-tolerance parts in the other resin without changes. Treat a material change as a new approval with samples and testing.
Where each is typically used
| Typically acetal | Typically nylon |
|---|---|
| Precision gears and small mechanisms | Heavy-duty gears and sprockets |
| Valve and pump components | Rollers, wheels and wear pads |
| Fixtures, jigs and close-fit parts | Structural brackets (glass-filled) |
| Clips and snap fits needing spring-back | Bushings in dirty or shock-loaded service |
| Parts in wet or humid environments | Parts near heat such as motors |
Common mistakes
- Specifying nylon for a precision part in a humid environment, then fighting dimensional drift.
- Using acetal where strong acids or chlorinated cleaners are present.
- Ignoring bonding: acetal is hard to glue, so plan mechanical fastening.
- Writing only “nylon” or “acetal” on the drawing without a grade, so properties vary between suppliers.
Other materials to consider
- UHMW-PE for very low friction and abrasion resistance at lower temperatures.
- PBT for molded parts needing low moisture uptake and good electrical properties.
- PEEK when temperature or chemicals exceed both.
Testing before production
Datasheets compare standard test bars, not your part. For gears and bushings, run samples at the real load, speed, temperature and humidity, and measure wear and fit after a meaningful run time. Check noise as well: gear pairs in different materials can run noticeably quieter or louder. For snap fits and clips, test repeated assembly cycles at the lowest expected temperature, where both materials are least forgiving. Machined prototypes are a quick way to compare both materials side by side before choosing which to mold.
How to decide
- Tight tolerances in changing humidity: start with acetal.
- Shock loads, abrasion or higher temperature: start with nylon.
- Structural stiffness with heat: glass-filled nylon.
- Gear pairs: consider acetal running against nylon.
- Test in the real environment before committing to production tooling.
Frequently asked questions
Is acetal or nylon better for gears?
Both are used. Acetal is preferred for precision and dimensional stability; nylon for shock loads and abrasion. Acetal-on-nylon pairs are common.
Why does nylon change size?
It absorbs moisture from the air and grows slightly, becoming tougher and less stiff. Acetal absorbs very little.
Which machines better, acetal or nylon?
Acetal machines more cleanly and holds tighter tolerances; nylon machines well but burrs more and moves with moisture.
Which handles higher temperatures?
Nylon, especially PA66 and glass-filled grades, generally handles higher temperatures than acetal.
Is Delrin the same as acetal?
Delrin is a trade name for acetal homopolymer. Acetal copolymers are sold under other names.