Liquid silicone rubber (LSR) and thermoplastic elastomers (TPE) are the two most common choices for molded soft parts: seals, gaskets, grips, buttons, valves, membranes and soft overmolds. They can look and feel similar, but they are different kinds of material. LSR is a thermoset silicone that cures in a heated mold; TPE is a thermoplastic that melts and solidifies like other plastics. That difference drives temperature range, compression set, tooling, cycle time, recyclability and cost. This guide compares them so you can choose before tooling. For processing details see LSR molding and TPE.

Elastomer seals and soft-touch molded parts

Quick comparison

Factor LSR TPE
Material typeThermoset silicone (cured, cannot be remelted)Thermoplastic (can be remelted and recycled)
Temperature rangeVery wide, both high and lowNarrower; softens at elevated temperature depending on type
Compression setGenerally low; seals keep sealing force wellHigher in many grades; seals can take a set over time, TPV grades better
Hardness rangeSoft to medium-firmVery soft to semi-rigid
Chemical and UVGood UV and ozone resistance; swells in some oils and fuelsVaries by type; some grades good with oils, others not
Biocompatible / food gradesWidely available (check documentation per grade)Available for some grades (check documentation)
ToolingPrecision tools with tight shut-offs to avoid flash, cold runner systemsStandard thermoplastic tooling
CycleCure time in hot mold; sometimes post-cureCooling time; usually no post-process
OvermoldingPossible onto heat-resistant substrates with selected gradesVery common onto PP, ABS, PC, nylon with matched grades
CostHigher material and tooling costLower material and tooling cost

Temperature and long-term sealing

LSR keeps its elasticity across a wide temperature range, from cold to well above where most thermoplastics soften. It also tends to recover well after compression, so seals and gaskets keep their sealing force over time. TPE softens at elevated temperatures, and many grades take a compression set under sustained load, especially when warm. For seals near heat, in ovens, lighting, engines or sterilization, LSR or another rubber is usually the safer choice. For grips and covers at room temperature, TPE is often enough.

Tooling and cost

LSR is injected as a low-viscosity liquid that flows into very fine gaps, so tools must have precise shut-offs to avoid flash, and they usually use cold runners to keep material from curing before it reaches the cavity. That makes LSR tools more expensive than equivalent thermoplastic tools. TPE runs in standard thermoplastic tooling and machines. LSR material also costs more per kilogram. At high volumes, LSR’s automated, flashless production can still be competitive, but for most consumer grips and soft-touch parts, TPE is cheaper.

Get a quote for LSR or TPE parts

Overmolding and two-material parts

TPE is the standard choice for soft-touch overmolding on rigid plastics. Different TPE families bond to different substrates, so the TPE grade must be matched to the substrate (for example PP, ABS, PC or nylon). LSR can be overmolded too, onto substrates that tolerate its cure temperature, often using self-bonding LSR grades or primers. It is used where silicone’s properties are needed in a two-material part, such as sealed housings and medical-style devices. See overmolding.

Feel, appearance and wear

LSR has a smooth, dry silicone feel, can be clear or colored, and resists staining in many applications. TPE can be made with a wide range of textures and feels, matte or glossy, and in many colors. Some TPEs become sticky or chalky with age or with exposure to skin oils, sunscreen or cleaners; grade choice matters. LSR can attract dust and lint and tears more easily than some TPEs at sharp edges; good design with radii helps.

Recyclability and scrap

TPE runners and rejects can often be reground and reused, and parts can be recycled with suitable streams. LSR, as a thermoset, cannot be remelted; scrap is generally not reused in the same process. LSR tools are often designed for minimal waste with cold runners for that reason.

Design differences

  • Flash: LSR flows into gaps that TPE would not, so parting lines and vents are designed to tighter limits; TPE is more forgiving.
  • Undercuts: both soft materials can often be stripped off undercuts without side actions, which simplifies tools.
  • Wall thickness: LSR handles very thin walls and membranes; TPE thin walls are possible but flow length is more limited.
  • Shrinkage: both shrink, and LSR shrink continues during any post-cure; tools must allow for it.
  • Bonding to inserts: TPE bonds by melt compatibility; LSR needs self-bonding grades or primers.

Testing before committing

For seals, test compression set and sealing at the highest and lowest working temperatures and after aging. For grips and touch surfaces, test against skin oils, sunscreen and cleaners the product will meet. Prototypes can be made by vacuum casting or printing for feel, but compression set and chemical tests need the real material.

Prototyping

For LSR parts, compression-molded silicone or cast silicone prototypes are a common low-cost step before the LSR tool. For TPE parts, printed TPU or cast polyurethane can show shape and feel, and a prototype tool in aluminum can produce parts in the real TPE grade. Choose the route that matches what must be tested.

Where each is typically used

Typically LSR Typically TPE
Seals and gaskets exposed to heat or wide temperature swingsSoft-touch grips on tools and devices
Baby-care, kitchen and medical-style parts (with grade documentation)Overmolded handles and bumpers
Valves and membranes needing low compression setConsumer seals and plugs at room temperature
Lighting lenses and optical parts (clear grades)Cable strain reliefs and grommets
Keypads with long lifeFeet, pads and anti-slip parts

Other materials to consider

  • TPU: tougher and more abrasion resistant than most TPEs; used for wear surfaces and cables.
  • TPV: thermoplastic with better compression set and heat resistance than general TPEs; common for automotive seals.
  • Compression-molded silicone: lower tooling cost than LSR for low volumes or large parts.
  • EPDM or FKM rubber: for weather or fuel and oil resistance in seals.

How to decide

  1. Heat, wide temperature range or long-term sealing force: start with LSR.
  2. Soft-touch overmold on a plastic part at room temperature: start with TPE.
  3. Tight budget and moderate volume: TPE, unless performance requires silicone.
  4. Need a silicone part but low volume: consider compression-molded silicone.
  5. Unsure: prototype both and test compression set, feel and chemical exposure.

Frequently asked questions

What is the main difference between LSR and TPE?

LSR is a thermoset silicone that cures in the mold and keeps elasticity over a wide temperature range; TPE is a thermoplastic that melts and solidifies, with lower cost and easier processing.

Is LSR better for seals?

For seals exposed to heat or long-term compression, LSR usually performs better. TPE or TPV can work for room-temperature seals.

Why is LSR tooling more expensive?

LSR flows into tiny gaps, so tools need precise shut-offs and usually cold runners to prevent flash and premature curing.

Can TPE be overmolded on plastic?

Yes, it is the standard soft-touch overmold material, provided the TPE grade is matched to the substrate.

Can LSR be recycled like TPE?

No. LSR is a thermoset and cannot be remelted; TPE scrap can often be reground.

Get a quote for LSR or TPE parts

Send us your drawing

A real engineer reads every request and comes back with questions or a plan for quoting.

ProteForm short RFQ

Or message us on WhatsApp.

Send Drawings
Chat on WhatsApp