FKM fluoroelastomer, often sold as Viton among other trade names, is the seal material engineers reach for when nitrile is not enough: hotter oil, aggressive fuels, many acids and solvents. It costs several times more than nitrile and has weaknesses of its own, including poor low-temperature flexibility in standard grades and attack by some ketones, amines and hot water or steam. This page explains FKM types and how to specify FKM seals and molded parts.
What FKM is and where it fits
FKM is a family of fluorinated synthetic rubbers. Standard types differ mainly in fluorine content: higher fluorine generally improves chemical and fuel resistance but can reduce low-temperature flexibility. Cure system matters too. Bisphenol-cured compounds are common for O-rings and give good compression set, while peroxide-cured compounds often handle steam and hot water better. Low-temperature grades exist for cold service.
FKM is not the same as FFKM (perfluoroelastomer), which is a more expensive class for the most aggressive chemicals and temperatures. On the elastomers page FKM sits above nitrile in heat and chemical resistance and next to silicone, which handles wider temperatures but not fuels.
Properties you can plan around
FKM offers high continuous temperature capability, excellent resistance to oils, fuels, many aliphatic and aromatic hydrocarbons, many acids and chlorinated solvents, and excellent ozone and weathering resistance. Good grades have low compression set at temperature and low gas permeability, and some are used in vacuum equipment for low outgassing.
Limits: FKM is expensive. Standard grades stiffen in the cold, so check the minimum temperature. Ketones, low-molecular-weight esters, some amines, hot water and steam (for some cure systems), and certain glycol brake fluids can attack it. Tear and abrasion resistance are moderate, so dynamic seals need care. It is denser than most rubbers, which affects cost per part.
| If your part needs… | FKM is usually… | Talk to us about… |
|---|---|---|
| Hot oil, fuel or aggressive hydrocarbons | A strong candidate. | Fluid, temperature and fluorine level. |
| Service in the cold | Grade dependent. | Low-temperature FKM types or alternatives. |
| Steam or hot water | Grade dependent. | Peroxide-cured FKM or EPDM. |
| Ketones or amines | Often unsuitable. | EPDM, FFKM or a chemical review. |
| Lowest cost | Weak. | Nitrile or HNBR if the conditions allow. |
Send drawings for an FKM seal quote
Typical applications for FKM fluoroelastomer
These are places where FKM fluoroelastomer is typically used and why. They are general examples, not projects or customers of ProteForm. Images are generic illustrations.

Fuel system and engine seals
Why this material: Resists hot fuels, oils and many chemicals where nitrile would harden or swell.
Usual process: compression molding, injection molding

Chemical pump and valve seals
Why this material: Broad chemical resistance and heat resistance for process equipment.
Usual process: compression molding, transfer molding
High-temperature O-rings and gaskets
Why this material: Serves continuously at temperatures well above nitrile and EPDM in suitable grades.
Usual process: compression molding
Semiconductor and vacuum equipment seals
Why this material: Low outgassing and plasma or chemical resistance in specialty grades.
Usual process: compression molding
Processes we can coordinate for FKM parts
FKM parts are made by compression, transfer or injection molding, much like other rubbers, but usually with a post-cure in an oven to complete cross-linking and stabilize compression set. Flash is controlled by tool design and by trimming or cryogenic deflashing. Extruded cord and profiles can be cut and joined for large seals.
We coordinate FKM molding through partner molders that run fluoroelastomer compounds and can supply compound documents. Many FKM seals go into machined housings or valve bodies made from high-performance plastics such as PEEK or PVDF; we can review those through CNC machining in the same project.
Design notes for FKM parts
- Use standard O-ring sizes where possible; custom tools for a premium compound add cost.
- State the full fluid list, including cleaning agents, and the temperature range including start-up in the cold.
- Note whether the seal is static or dynamic; dynamic seals may need a different compound.
- Specify hardness and color; brown and black are common, and color can identify compound in assembly.
- Allow for post-cure shrinkage in tight dimensions.
FKM compared with nitrile and silicone
| Question | FKM | Nitrile (NBR) | Silicone |
|---|---|---|---|
| Fuel and oil | Excellent | Very good at moderate temperature | Fair |
| Maximum continuous temperature | Very high | Moderate | Very high |
| Low-temperature flexibility | Fair (grade dependent) | Good | Excellent |
| Chemical range | Broad | Narrower | Moderate |
| Relative cost | High | Low | Medium |
If the fluid is ordinary mineral oil at moderate temperature, nitrile may do the job at much lower cost. For hot air or wide temperature swings without fuel, review silicone rubber. For water and steam, EPDM is often better than standard FKM.
What to put in your FKM RFQ
- Drawing or seal size and gland details.
- All media, temperature range and pressure.
- Hardness, color and any required FKM type or specification.
- Documents needed, such as material certificates or compliance statements for the compound.
- Quantities and whether a standard size could be used.
Frequently asked questions
Is FKM the same as Viton?
Viton is a brand name for FKM fluoroelastomers. Other suppliers sell FKM under other names. Specify the properties or standard you need rather than a brand alone.
What temperature can FKM handle?
FKM handles much higher continuous temperatures than nitrile or EPDM. The exact limit depends on the compound, so we confirm it with the compound data.
When should I not use FKM?
In ketones such as acetone, some amines, certain brake fluids, and steam or hot water for some cure systems, and when cold flexibility matters with standard grades.
What is the difference between FKM and FFKM?
FFKM is perfluorinated, more chemically resistant and much more expensive. It is used where FKM is attacked, such as some semiconductor and chemical processes.
Why are FKM parts post-cured?
Post-cure completes the cross-linking, which improves compression set and stability at temperature.