PEEK and PEI are both high-performance thermoplastics used where ordinary engineering plastics run out of heat resistance, strength or flame performance. They are often shortlisted together and then chosen for very different reasons. PEEK is semi-crystalline and is chosen for high continuous temperature, chemical resistance and wear; PEI (often sold as Ultem) is amorphous and is chosen for strength, dimensional stability and inherent flame resistance at a lower cost. This guide compares them for machined and molded parts. Values depend on grade and fillers; compare datasheets for the grades you are considering.
Quick comparison
| Property | PEEK | PEI |
|---|---|---|
| Structure | Semi-crystalline | Amorphous |
| Appearance | Opaque, tan or black | Transparent amber in unfilled grades; opaque when filled |
| Continuous temperature | Higher of the two | High, but generally below PEEK |
| Chemical resistance | Very broad, including many solvents, fuels and hot water | Good with many chemicals; attacked by some solvents such as chlorinated hydrocarbons; can stress-crack |
| Wear and friction | Very good, especially bearing grades with PTFE, carbon or graphite | Moderate; not usually chosen for wear |
| Flame behavior | Inherently flame resistant, low smoke | Inherently flame resistant, low smoke; widely used in aircraft interiors |
| Dimensional stability | Good; annealing helps machined parts | Very good; low shrinkage and creep for an amorphous resin |
| Sterilization | Withstands repeated steam sterilization in many grades | Withstands some sterilization methods; check the grade |
| Relative cost | Higher | Lower than PEEK, still high compared with engineering plastics |
Heat and long-term performance
PEEK keeps useful mechanical properties to higher continuous temperatures than PEI, and its semi-crystalline structure helps it resist creep and chemicals at temperature. PEI has a high glass transition temperature and holds stiffness well up to near that point, then softens more abruptly, as amorphous plastics do. For parts that live in hot oil, steam or hot chemicals for long periods, PEEK is usually the safer starting point. For parts that see high temperature but mild chemicals, PEI is often enough.
Chemicals and stress cracking
PEEK resists a very wide range of chemicals, which is why it appears in pumps, valves, seals and semiconductor equipment. PEI resists many fluids, including some automotive fluids and cleaning agents, but certain solvents attack it, and stressed PEI parts can crack in contact with them. If a part is wiped with cleaners, sprayed with fluids or bolted under load, test it with the real chemicals.
Wear and bearing parts
PEEK is a common choice for high-temperature bushings, thrust washers, seal rings and wear pads, often in bearing grades filled with PTFE, graphite and carbon fiber. PEI is not usually chosen for sliding wear. If the part slides or rotates against metal under load, PEEK or another bearing material is generally the better fit.
Get a quote in PEEK or PEI
Flame, smoke and interiors
Both are inherently flame resistant with low smoke. PEI is widely used for aircraft interior components and electrical parts where flame, smoke and toxicity requirements apply, partly because it costs less than PEEK and molds well into thin-walled parts. Whether a specific grade meets a specific requirement depends on the grade, thickness and test; name the requirement and we check documentation from the factory. We make no certification claim here.
Machining PEEK and PEI
- Both machine well from rod and plate with sharp tools and controlled heat.
- PEEK stock and parts are often annealed for tight tolerances because internal stress can cause movement after machining.
- PEI machines cleanly and holds size well; avoid coolants or cleaning agents that can attack it.
- Filled grades of both, especially carbon-fiber, wear tools faster.
- Material cost is significant for both, so near-net stock sizes and nesting matter.
See our CNC machining page.
Molding PEEK and PEI
Both can be injection molded, but they need high melt and mold temperatures and equipment set up for them. PEI molds readily into thin walls and fine detail and is common for molded electrical and interior parts. PEEK molding is more demanding and the resin is expensive, so molding usually makes sense at higher volumes. Both need thorough drying. See injection molding.
Filled grades
| Grade type | PEEK | PEI |
|---|---|---|
| Glass-filled | Stiffer, more stable, common for structural parts | Stiffer and more stable; common for molded structural and electrical parts |
| Carbon-fiber filled | Highest stiffness and strength; used to replace metal | Available; less common |
| Bearing grades (PTFE, graphite, carbon) | Widely used for wear parts | Rarely used |
| Unfilled | Best toughness and chemical resistance | Transparent amber, best for clear or electrical parts |
Fillers change stiffness, wear, shrinkage and machinability, and they can make properties direction-dependent in molded parts. Specify the filled grade on the drawing, not only the base polymer.
Replacing metal with PEEK or PEI
Both are used to replace aluminum or stainless steel parts for weight, corrosion or insulation reasons. A direct copy of a metal design rarely works: plastics are less stiff, creep under sustained load and expand more with heat. Thicker sections, ribs, inserts for threads and allowance for thermal expansion are usually needed. Prototype in the chosen grade and test under load and temperature.
Where each is typically used
| Typically PEEK | Typically PEI |
|---|---|
| Bushings, seal rings and thrust washers in hot or chemical service | Aircraft interior parts and brackets (non-structural) |
| Pump and valve components | Electrical connectors and insulators |
| Semiconductor and analytical equipment parts | Sterilizable instrument handles and trays (check grade) |
| Components in steam or hot water | Thin-walled housings needing flame resistance |
| High-load parts replacing metal | Fixtures and manifolds needing stiffness and stability |
Other materials to consider
- PPS: high heat and chemical resistance at lower cost than PEEK, more brittle.
- PPSU: amorphous, tough, excellent repeated sterilization; often compared with PEI for medical-style parts.
- PEKK: in the same family as PEEK with different processing behavior.
- PAI: very high strength and wear at temperature, mostly machined.
Cost and supply
Both resins are expensive, and stock shapes in large sizes can have long supply times depending on region and grade. For machined parts, material is often a large share of the price, so nesting parts in plate and choosing stock close to finished size matters. For molded parts, resin cost per part is high, which makes scrap and runner waste costly; hot runners or small runners are often considered. Ask suppliers to confirm stock availability before committing to a schedule.
How to decide
- If the part slides, wears or lives in aggressive chemicals or steam, start with PEEK.
- If it needs high stiffness, stability and flame performance with mild chemicals, start with PEI.
- If cost is the constraint and both are technically acceptable, PEI is usually lower.
- Test with the real chemicals, temperatures and loads before committing.
See our high-performance plastics hub for related materials.
Frequently asked questions
Is PEEK better than PEI?
For continuous high temperature, chemical resistance and wear, PEEK usually performs better. PEI offers excellent strength, stability and flame resistance at lower cost.
Why is PEI used in aircraft interiors?
It is inherently flame resistant with low smoke and molds well into thin parts at lower cost than PEEK. Specific requirements still need grade documentation.
Which is easier to machine, PEEK or PEI?
Both machine well. PEEK often needs annealing for tight tolerances; PEI holds size well but must be kept away from aggressive solvents.
Is PEI transparent?
Unfilled PEI is transparent amber. PEEK is opaque.
Which costs more?
PEEK generally costs more than PEI, both as resin and as stock shapes.