Your enclosure is drawn in ABS, or about to be, and someone on the team has asked whether it should be PC/ABS. The blend is tougher and handles heat better, but it costs more and it’s fussier to mold. This page compares ABS vs PC/ABS for electronic enclosures, so you can decide on the housing you actually have rather than on a datasheet.
Generic illustration, not a part ProteForm made.
What actually changes when you move from ABS to PC/ABS?
PC/ABS is a blend of polycarbonate and ABS. It borrows impact strength and heat resistance from the PC side and keeps much of the easy molding and good surface of the ABS side. For an enclosure, that usually shows up in four places: how the housing survives a drop, especially when it’s cold; how it holds shape near warm electronics; whether a flame rating is reachable at the wall thickness you want; and how much each part costs.
There’s a catch on each side. PC/ABS needs drying before molding, which ABS also benefits from but tolerates better; our resin drying page explains why that matters. PC/ABS can stress crack when some cleaners, oils, or threadlockers meet a loaded feature. And the word covers a family of grades, some closer to ABS and some closer to PC, so two “PC/ABS” quotes may not be quoting the same material.
For the material background, see our ABS and PC/ABS pages. If you’re weighing pure polycarbonate instead, PC vs ABS covers that comparison.
| Enclosure question | ABS | PC/ABS |
|---|---|---|
| Drop and impact, including in the cold | Good for most indoor products | Usually better, which is the main reason people switch |
| Near a power supply, battery, or LED driver | Can soften or creep if it runs warm | Holds shape at higher temperatures, depending on grade |
| Flame rating at thin walls | Flame-retardant grades exist; check the rating at your thickness | Flame-retardant grades often reach a rating at thinner walls; check the specific grade |
| Cleaners, hand sanitizer, oils | Attacked by some solvents | Can stress crack with some chemicals on loaded features |
| Molding | Easy, wide process window | Needs drying and tighter process control |
| Paint, print, texture | Very good | Very good |
| Decorative plating | Long-established on plating grades | Plating grades exist; fewer options |
| Material cost | Lower | Higher |
When is ABS enough for an electronic enclosure?
More often than people expect. A desktop device, a wall-mounted controller indoors, a remote, a meter that lives in a drawer: if the housing stays near room temperature, doesn’t get dropped much, and either needs no flame rating or can meet it with a flame-retardant ABS grade at your wall, ABS is a sensible default.
It molds easily, it takes texture and color well, and it’s cheaper per kilogram. On a cost-sensitive product with modest volume, that difference adds up over every shot. ABS is also easy to get as machinable stock and as print material, which helps when you prototype the enclosure before tooling.
If ABS cracked in testing, look at the design before blaming the resin. A sharp corner at the root of a screw boss or a snap hook flexed past its limit will crack in either material. Our guides on snap-fit design and wall thickness cover the usual causes.
When does PC/ABS earn its extra cost?
The blend pays for itself when the housing has a job ABS struggles with. Handheld products that get dropped on hard floors are the classic case, and the cold makes it worse because ABS gets more brittle as temperature falls. Chargers, adapters, and housings around a hot board are another, where you need the walls to stay stiff and the bosses to keep holding screws after months of warm running.
Thin walls with a flame rating are the third. If your product needs a particular flammability rating and you’re trying to keep walls thin for weight or size, some flame-retardant PC/ABS grades get there at thinner sections than many ABS grades. That’s grade-specific, so compare the actual listings rather than the family name.
If none of those apply, the switch may add cost without fixing anything. Be clear about which problem you’re solving before you change the material on the drawing.
Send drawings for an enclosure molding quote
Send the CAD, the drawing, what the enclosure has to survive, and any flame rating you need. We’ll review the design, check whether ABS or PC/ABS fits, confirm a molder who runs that material, and only then quote.
How does a flame rating change the choice?
Flammability ratings such as UL 94 belong to a specific resin grade, in a specific color, at a specific thickness. They don’t belong to “ABS” or “PC/ABS” in general. Before you pick a material, check the listing for the exact grade and make sure your thinnest relevant wall is at or above the listed thickness, in the color you plan to use.
Two practical points. First, a material rating isn’t a product certification. Your finished device may still need its own safety testing, and that’s between you and your test lab. Second, once a grade is approved, lock it in the drawing or the purchase order, along with the color. A molder swapping to a “similar” flame-retardant grade can leave you with parts that no longer match your safety file. We name the grade in our quotes, so any substitution has to come back to you.
Can the same mold run ABS and PC/ABS?
Sometimes, and it’s a common question when a product already in ABS needs to get tougher. The shrink of the two materials is in a broadly similar range, so a tool built for one may produce usable parts in the other. Broadly similar isn’t identical, though. Dimensions can shift, especially on long or thin features, and the melt and mold temperatures differ.
The tool may need venting or cooling changes, and the gate that worked for ABS may leave more visible marks or molded-in stress with PC/ABS. Gloss and texture can look a little different, and a color matched in ABS will need to be matched again; see plastic color matching.
So treat a material change as a new approval. Run samples, measure them, test them in your assembly, and repeat any drop or flame testing that depended on the old material. If a tool is still being designed, tell the toolmaker which material it’s for, or ask for it to be designed so that either can be trialed.
Which design details matter more than the resin?
On most enclosures, the details decide whether parts crack, not the material name. Generous radii at boss roots and inside corners, uniform walls, ribs that don’t make thick spots, and snap fits sized for the strain the grade allows all matter in both materials.
Screw bosses deserve special attention with PC/ABS. Thread-forming screws designed for plastics, or brass inserts placed by heat or by insert molding, reduce stress at the boss. Check every threadlocker, lubricant, gasket, and adhesive that touches the housing, because those are the usual triggers of chemical cracking. Both materials weld well, so if the halves will be joined permanently, ultrasonic welding is worth designing in from the start.
When are we not the right fit?
If the enclosure lives outdoors in sunlight, neither ABS nor standard PC/ABS is a good first choice without paint or a stabilized grade; look at ABS vs ASA. If you need a clear window, that’s polycarbonate or acrylic, not either of these. If you need heavy shielding or heat spreading, a metal housing may simply be the better design.
If you need a handful of housings, molding probably isn’t the answer yet. Printed, machined, or vacuum cast enclosures can get you through early builds. And we don’t certify products. We can source a material with the rating you specify, but your product’s safety approval stays with you and your test lab.
How do we help with an enclosure material choice?
We work with a network of factories in China we know well. We review your enclosure for manufacturability, talk through ABS or PC/ABS against what the housing has to do, and match it to a molder who runs that material regularly. We confirm the supplier and the resin grade before we quote. You’ll find related programs on our electronics industry page and on consumer electronics parts.
For a quick, useful review, include:
- 3D CAD and a 2D drawing with critical dimensions and cosmetic faces marked
- The material you have now, or what the enclosure must survive: drops, heat, cleaners, sunlight
- Any flame rating, the thinnest wall where it applies, and the color
- Texture, paint, printing, or plating requirements
- How the halves join: screws, inserts, snaps, or welding
- Prototype and production quantities, and your target date
Frequently asked questions
Is PC/ABS stronger than ABS?
In impact, usually yes, especially at low temperature, and it keeps its shape at higher temperatures. It costs more and needs drying before molding. For an indoor, room-temperature housing, ABS is often enough.
Is PC/ABS worth the extra cost for an electronics enclosure?
It is when the housing gets dropped, runs warm, or needs a flame rating at thin walls. If none of those apply, ABS usually does the job at a lower material cost.
Can I switch an existing ABS mold to PC/ABS?
Often the tool can run it, but treat it as a new approval. Dimensions, cosmetics, and color can change, and the tool may need venting, cooling, or gate adjustments. Repeat any testing that depended on the old material.
Does PC/ABS make my product flame rated?
No. A flame rating belongs to a specific grade, color, and thickness of material. Your finished product may need its own safety testing, which is separate from the material listing.
Why did my PC/ABS housing crack at the screw bosses?
Common causes are a cleaner, lubricant, or threadlocker on a stressed boss, sharp corners at the boss root, overtightened screws, and high molded-in stress. Check chemical contact and the boss design before changing material.
Send drawings for an ABS or PC/ABS enclosure quote
Send the CAD, drawing, quantities, and what the housing has to survive. We’ll review the design, confirm the material grade and a molder who runs it, and quote with the assumptions written down. No instant quotes.