Polycarbonate gets picked when a part has to be clear and tough at the same time: a sensor window, a light cover, a machine guard, a housing that must survive a drop. It does those jobs well. It also cracks if it meets the wrong cleaner, scratches more easily than acrylic, and punishes a mold or a drawing that ignores its quirks. This page covers what you should know before you put “PC” on a drawing, and what we check when we review custom polycarbonate parts for molding, machining or forming.
Why do engineers choose polycarbonate?
PC is an amorphous engineering plastic with a useful mix of properties: high impact strength, good clarity in natural grades, decent heat resistance for a transparent plastic, and good dimensional stability because it doesn’t crystallize as it cools. It machines cleanly, molds well with the right process, and thermoforms from sheet. Flame-retardant, UV-stabilized, glass-filled and optical grades are available. If you need a UL 94 flame rating, name the designation, the thinnest wall, and the color; the rating is tied to a specific grade, not to PC as a family. If you need a UL 94 flame rating, name the designation, the thinnest wall, and the color; the rating is tied to a specific grade, not to PC as a family.
Those are family traits. Real numbers belong to a specific grade from a specific supplier, so we confirm the grade and its data sheet on each project rather than quoting family values. If you are still comparing families, the engineering plastics page puts PC next to nylon, POM, PBT and acrylic.
Where does polycarbonate let you down?
Most PC problems we see on drawings come from one of these, and each one is easier to handle before the tool is cut.
Chemical stress cracking. PC can crack when certain chemicals meet a part that is under stress. Some solvents, oils, aggressive cleaners, threadlockers and plasticized materials touching the part are common causes. The stress can come from the load in use, from a press-fit, or from the molding itself. Tell us every chemical the part will see, including the cleaner your customer will wipe it with. That single line in an RFQ saves more failed parts than any other.
Notch sensitivity. PC is tough, but a sharp internal corner concentrates stress and can turn a tough part into a brittle one. Put radii on internal corners, at the base of ribs and bosses, and around holes.
Scratches. Uncoated PC scratches more easily than acrylic or glass. For windows and lenses that get wiped, ask about a hard coat, or consider whether acrylic (PMMA) fits better when impact is less important.
UV and outdoor use. Standard PC can yellow and lose toughness in sunlight. Outdoor parts need a UV-stabilized grade or a protective coating. Say whether the part lives indoors or outdoors.
Hot water and steam. Long exposure to hot water can degrade PC. If the part is washed hot or steam-cleaned, say so; another resin may be safer.
| If your part needs… | PC is usually… | Talk to us about… |
|---|---|---|
| Clarity and impact strength together | A strong candidate. | Optical grade, gate location, polish and coating. |
| Scratch resistance on a clear face | Weak without a coating. | Hard coat, or acrylic if impact is modest. |
| Outdoor life | Only with UV protection. | UV-stabilized grade or coating, and color. |
| Contact with oils, solvents or strong cleaners | Risky. | The exact chemicals, residual stress, or PC/PBT or another resin. |
| Flame rating such as UL 94 | Possible with FR grades. | Rating, thickness and grade; documents are grade-specific. |
| Higher stiffness | Possible with glass-filled grades. | Loss of clarity, more warpage risk, wear on the tool. |
Send drawings for a polycarbonate parts quote
Typical applications for Polycarbonate (PC)
These are places where Polycarbonate (PC) is typically used and why. They are general examples, not projects or customers of ProteForm. Images are generic illustrations.

Sensor and camera windows
Why this material: Clear and impact resistant; optical and coating needs are agreed per project.
Usual process: injection molding; CNC machining for prototypes

Machine guards and safety covers
Why this material: High impact strength in a transparent sheet.
Usual process: thermoforming, CNC machining

Electronic housings and light covers
Why this material: Toughness, heat resistance and flame-retardant grades for enclosures.
Usual process: injection molding

Aircraft cabin covers and lenses (non-structural)
Why this material: Light weight and toughness; flammability documents are grade-specific.
Usual process: injection molding, thermoforming
What changes when you injection mold polycarbonate?
PC has to be dried properly before molding. Moisture left in the pellets breaks down the material in the barrel and shows up as splay, bubbles or brittle parts. It also needs higher melt and mold temperatures than many commodity resins, and its melt is stiff, so long thin flow paths are hard to fill. Gate size and location matter more than usual, especially on clear parts, where a gate blush or flow line sits in plain view.
Molded-in stress is the hidden problem. A part that looks perfect can carry enough stress to crack later when it meets a chemical or a screw. Uniform walls, generous radii, enough draft and a sensible gate all help. Some shops anneal critical parts after molding, and some use a solvent dip test on samples to reveal stress. Ask for that check if the part will be exposed to chemicals in use.
For clear parts, the mold surface becomes the part surface. Mark which faces must be optically clear, and expect those faces to need a high polish on the tool. Ejector pins, gates and parting lines need to stay off them. Our injection molding page covers what we review on any molding project, and the sealed PC fluid manifold review walks through moving a layered PC part from machined prototypes to molded layers.
Machining or thermoforming PC instead
CNC machining PC from sheet or rod suits prototypes, low volumes and thick parts. It cuts well, but machining leaves stress and a frosted surface. Clear machined parts need polishing, and some shops anneal parts that will be bonded, solvent-cleaned or loaded. Coolants and cleaners used in the shop must be PC-compatible, for the same stress-cracking reason as above.
For large, fairly simple shapes such as covers, guards and windows, thermoforming PC sheet can be much cheaper in tooling than a mold. PC sheet must be dried before forming or it bubbles. The finish on the non-tool side and the thickness variation over deep draws should be discussed before you choose the route.
PC blends and filled grades
Blends adjust PC’s weak points. PC/ABS is common for housings: easier to process, good impact, and less sensitive to notches than pure PC, but it isn’t clear. PC/PBT improves chemical resistance and is often seen in parts exposed to fluids. Glass-filled PC adds stiffness and reduces creep but gives up clarity, can warp along the fiber direction, and wears the tool faster. Which one fits depends on your loads, chemicals and appearance needs, and we confirm the grade with the material supplier and the molder.
Clear PC windows and optical parts
For sensor windows, light guides and lenses, the questions get sharper: which wavelengths matter, how much haze is acceptable, what coating is needed, and how the part will be measured. We published a separate note on what to define for polycarbonate LiDAR windows that covers those points in more detail. We won’t promise optical performance that hasn’t been specified and tested on your geometry.
What should your polycarbonate RFQ include?
- 3D CAD and a 2D drawing with critical dimensions and tolerances.
- Grade if you have one, or the properties you need: clarity, flame rating, UV, stiffness.
- Every chemical the part will touch, including cleaners, oils, adhesives and threadlockers.
- Indoor or outdoor use, temperature range and any hot water or steam.
- Optically clear faces, cosmetic faces, and coating or hard coat requirements.
- Assembly method: screws, press-fits, snap fits, bonding or welding.
- Quantity now and later, which decides between machining, forming and molding.
- Documents you need for the grade. A blank RFQ checklist is on our downloads page.
Frequently asked questions
Is polycarbonate stronger than acrylic?
PC has much higher impact strength than acrylic (PMMA), which is why it is used for guards and covers that may be hit. Acrylic is more scratch resistant and often clearer. Choose based on whether impact or surface wear matters more for your part.
Why did my polycarbonate part crack?
Common causes are chemical stress cracking from a cleaner, oil, solvent or adhesive, sharp internal corners, molded-in stress, or a press-fit that overloads a boss. Send the part, what it touched and where it cracked, and we can help find the likely cause before the next run.
Can polycarbonate be used outdoors?
Yes, with a UV-stabilized grade or a protective coating. Standard grades can yellow and lose toughness in sunlight over time.
Does polycarbonate need to be dried before molding?
Yes. PC absorbs moisture, and wet material degrades during molding, causing splay, bubbles and brittle parts. Drying is a normal step and is checked as part of process control.
Should I use PC or PC/ABS for an enclosure?
PC/ABS is often chosen for opaque enclosures because it is easier to mold and less notch-sensitive, while pure PC is used when clarity or higher heat resistance is needed. Your loads, chemicals, flame rating and appearance decide it.