Custom manufacturing support for product teams worldwide Discuss Your Project  →

PC vs PETG

Resources / PC vs PETG

Polycarbonate and PETG are both clear, tough plastics used for guards, covers, displays, trays and enclosures, and they are often quoted as alternatives, especially in sheet. Polycarbonate is tougher and handles more heat; PETG is easier to form and fabricate, often has better chemical resistance to common cleaners, and usually costs less. This guide compares them on toughness, heat, forming, fabrication, chemical behavior and cost, and explains where each is typically used.

Thermoformed clear plastic trays and housings

Quick comparison

Property Polycarbonate (PC) PETG
Impact strengthVery highHigh, but lower than PC
Heat resistanceHigherLower; softens at modest temperatures
ClarityVery goodVery good
ThermoformingNeeds pre-drying; higher forming temperatureOften formed without pre-drying; forms at lower temperature
Cutting and bendingTough; cold-bendableEasy to cut, die-cut, cold-bend
Chemical resistanceSensitive to many solvents and some cleanersOften better with common cleaners
UV resistanceNeeds UV-stabilized grade or coatingNeeds UV-stabilized grade for outdoor use
Flame-rated gradesWidely availableAvailable, less common
CostHigherLower
Often sold asLexan, MakrolonVivak, Spectar and other copolyester sheets

Toughness

Polycarbonate is among the toughest transparent plastics and is used for machine guards, safety shields and protective covers that must withstand impact. PETG is also tough, much tougher than acrylic, and is adequate for many covers, displays and guards that see moderate abuse. If impact resistance is the primary requirement, such as a guard that may be struck by a tool or debris, PC is the safer choice. If the part needs to be clear, reasonably tough and inexpensive, PETG often suffices.

Heat

PC keeps its shape at much higher temperatures than PETG. PETG softens at relatively modest temperatures, which rules it out near lights, motors, heaters or in hot vehicles, and for parts that must be cleaned with hot water. PC handles these better. For indoor parts at room temperature, PETG’s lower heat resistance is rarely a problem.

Forming and fabrication

PETG is one of the easiest materials to thermoform. It forms at lower temperatures, reproduces mold detail well and is often formed without pre-drying, which shortens lead time and reduces cost. PC usually must be dried before forming to avoid bubbles, needs higher forming temperatures and is less forgiving. PETG also cuts, routes, drills and die-cuts cleanly and can be cold-bent. PC can also be cold-bent and machined, but its toughness makes some cutting operations slower. See thermoforming and polycarbonate thermoforming.

Send your clear part for a material review

Chemical resistance

PC is prone to stress cracking with many solvents, some cleaning agents, adhesives and lubricants, particularly around screws or bends. PETG generally tolerates common cleaners and disinfectants better, which is one reason it is used for displays, store fixtures and protective screens that are cleaned often. Neither is suitable for aggressive solvents. Always check the specific cleaning agents against supplier data and test on stressed samples.

Molding and printing

Both can be injection molded. PC is the more common molding resin for clear, tough, heat-resistant parts; PETG and other copolyesters are used for clear consumer and packaging-type parts. Both are hygroscopic and must be dried before molding. In 3D printing, PETG is one of the most popular FDM filaments because it prints easily with little warp; PC is harder to print, needing higher temperatures and an enclosed printer. See injection molding and 3D printing.

Where each is typically used

Application Usual choice Why
Machine guards and safety shieldsPCImpact resistance
Retail displays, store fixtures, sneeze guardsPETGCost, easy fabrication, cleaner resistance
Thermoformed clear trays and coversPETGEasy forming, cost
Clear covers near heat sources or lightsPCHeat resistance
Electrical enclosure windowsPCToughness, flame-rated grades
Point-of-sale and signagePETG or acrylicCost, appearance

Outdoor use

Standard grades of both yellow and lose toughness with long UV exposure. UV-stabilized PC sheet, often with a co-extruded UV layer on one or both faces, is widely used for outdoor glazing and covers; make sure the UV face is installed facing out. UV-resistant PETG grades exist but are less common. For long outdoor life, compare manufacturer weathering data and warranty terms for the specific sheet.

Coatings, printing and bonding

Uncoated PC scratches easily, so hard-coated PC sheet is used for parts that are wiped often or exposed to abrasion. PETG also scratches, and hard-coated grades are available. Both can be screen printed and digitally printed for displays. Both can be solvent-bonded or adhesive-bonded, but PC is more prone to stress cracking from solvents, so test the adhesive on stressed samples. Mechanical fastening should use oversized holes and avoid over-tightening.

Thickness and stiffness

Both are less stiff than metal and glass, so large flat panels deflect. Increasing thickness, adding formed ribs or flanges, or supporting edges with a frame keeps panels flat. Because PETG is somewhat less tough, guards that must stop impacts may need thicker PETG than PC for comparable performance, which can narrow the cost gap. Compare cost at the thickness each material actually needs.

Alternatives

  • Acrylic: better scratch resistance and weathering, but brittle; see acrylic vs polycarbonate.
  • PET: clear, used for packaging and formed trays.
  • COC/COP: very low moisture, optical and lab-type parts.
  • SAN: clear, rigid, lower cost for consumer parts.

Cost

PETG sheet and resin are usually less expensive than PC, and easier forming and fabrication can reduce labor further. For guards that must meet impact requirements, PC’s extra cost buys real performance. For displays, covers and trays, PETG often gives the best value. Compare quoted part prices, including forming, trimming and any coating.

For thermoformed parts, also consider the mold: PETG can often be formed on simpler, lower-temperature tooling, while PC benefits from temperature-controlled molds for consistent results. That difference can matter more than the sheet price on short runs. Forming lead time can also be shorter with PETG because there is no drying step before forming.

Both materials are also available in tinted, frosted and textured sheet. If a part needs privacy, glare reduction or diffused light, check which finishes are available in the thickness you need before choosing, because availability differs between the two and between sheet suppliers.

How to decide

  • High impact or safety function: PC.
  • Heat above room temperature: PC.
  • Large formed parts on a budget: PETG.
  • Frequent cleaning with common disinfectants: PETG is often more forgiving; test both.
  • Flame rating required: PC is more widely available in rated grades.

Specify the grade, sheet thickness, any UV or hard coating, the operating temperature and the cleaning regime when requesting quotes, so suppliers can quote truly comparable parts in either material.

Frequently asked questions

Is PETG as strong as polycarbonate?

No. PETG is tough, but PC has much higher impact strength.

Which handles heat better?

Polycarbonate. PETG softens at relatively modest temperatures.

Which is easier to thermoform?

PETG. It forms at lower temperatures and is often formed without pre-drying.

Which is cheaper?

PETG is usually less expensive than polycarbonate.

Which is better for sneeze guards and displays?

PETG is common because it is economical, easy to fabricate and tolerates many cleaners; PC is used where impact matters more.

Send your clear part for a material review

Send us your drawing

A real engineer reads every request and comes back with questions or a plan for quoting.

ProteForm short RFQ

Or message us on WhatsApp.

Send Drawings
Chat on WhatsApp